The insulator-metal transition temperature, Tim of Lal-x SrxMnO3 (x = 0.0, 0-05, 0.15 and 0.3) was studied during warming and cooling between 50 K to 300 K. The results showed that Tim of Lal-x SrxMnO3 shifted to a higher temperature as Sr was substituted for La. Scanning electron micrographs showed that the average grain size is in the range of 0.6 ?m - 1.4 ?m. Grain boundaries are almost completely revealed for x = 0.3. X-Ray powder diffraction patterns showed cubic structure (space group Pm-3m) and contain no secondary phases.