Failure investigation on reheater tube due to deposit and wall thinning

dc.citedby11
dc.contributor.authorPurbolaksono J.en_US
dc.contributor.authorTarlochan F.en_US
dc.contributor.authorRahman M.M.en_US
dc.contributor.authorNordin N.F.en_US
dc.contributor.authorAhmad B.en_US
dc.contributor.authorid8621252500en_US
dc.contributor.authorid9045273600en_US
dc.contributor.authorid55328831100en_US
dc.contributor.authorid26326390700en_US
dc.contributor.authorid36781813400en_US
dc.date.accessioned2023-12-29T07:55:49Z
dc.date.available2023-12-29T07:55:49Z
dc.date.issued2009
dc.description.abstractFailure analysis of a reheater tube showed that the failure was caused by overheating and wall thinning. Finite element modeling, dimensional measurements, and microscopic examinations were performed to investigate the root cause of the failure. Wall thinning, due to excessive coal-ash corrosion, and overheating, due to scale buildup on the tube were measured, and estimations, the average corrosion and scale growth rates, were made. The combination of excessive scale formation on the inner tube surfaces and wall thinning due to coal-ash corrosion on the outer tube surfaces combined to cause the failure of the reheater tube. � 2009 ASM International.en_US
dc.description.natureFinalen_US
dc.identifier.doi10.1007/s11668-009-9250-1
dc.identifier.epage369
dc.identifier.issue4
dc.identifier.scopus2-s2.0-70449523211
dc.identifier.spage365
dc.identifier.urihttps://www.scopus.com/inward/record.uri?eid=2-s2.0-70449523211&doi=10.1007%2fs11668-009-9250-1&partnerID=40&md5=9667abdb1fabe5c565ad4a465ff0e790
dc.identifier.urihttps://irepository.uniten.edu.my/handle/123456789/30916
dc.identifier.volume9
dc.pagecount4
dc.sourceScopus
dc.sourcetitleJournal of Failure Analysis and Prevention
dc.subjectBoiler material
dc.subjectDeposits
dc.subjectFailure analysis
dc.subjectHigh temperature
dc.subjectThinning
dc.subjectTube burst
dc.subjectBoiler deposits
dc.subjectBoilers
dc.subjectCorrosion
dc.subjectFailure analysis
dc.subjectMicroscopic examination
dc.subjectSafety factor
dc.subjectScale (deposits)
dc.subjectTubes (components)
dc.subjectBoiler material
dc.subjectDimensional measurements
dc.subjectFailure investigation
dc.subjectFinite element modeling
dc.subjectHigh temperature
dc.subjectInner tubes
dc.subjectReheater tubes
dc.subjectRoot cause
dc.subjectScale formation
dc.subjectThinning
dc.subjectTube burst
dc.subjectWall thinning
dc.subjectQuality assurance
dc.titleFailure investigation on reheater tube due to deposit and wall thinningen_US