Publication:
The effect of sintering temperature on the electrical and magneto-transport properties of magnetoresistive NSMO

dc.contributor.affiliationen_US
dc.contributor.authorAhmad Razikin Badroll Hisham
dc.date.accessioned2023-05-03T15:29:32Z
dc.date.available2023-05-03T15:29:32Z
dc.date.issued2015
dc.description.abstractThe effects of varying sintering temperature of 1150C, 1250C & 1350C on the electrical and magneto-transport properties of magnetoresistive Nd0.68Sr0.32MnO3 have been investigated. The samples were fabricated using Solid State Reaction method. The sample sintered at 1350C have the smallest grain size which is 27.5. As sintering temperature get higher almost all the grains become smaller. Besides, the sample sintered at 1350C has the largest MR value which is 1.2% and the largest T value of 118.36E10K. As sintering temperature get higher, the Tim get larger. The largest Tim value recorded in this research was 234K.en_US
dc.identifier.urihttps://irepository.uniten.edu.my/handle/123456789/20872
dc.language.isoenen_US
dc.subjectMagnetoresistanceen_US
dc.subjectManganese oxidesen_US
dc.titleThe effect of sintering temperature on the electrical and magneto-transport properties of magnetoresistive NSMOen_US
dc.typeResource Types::text::Thesisen_US