The effect of holding time on the mechanical and physical properties of titania-wollastonite-hydroxyapatite composites

dc.contributor.authorDinesh R.en_US
dc.contributor.authorMeenaloshini S.en_US
dc.contributor.authorSankar U.en_US
dc.contributor.authorid56740614600en_US
dc.contributor.authorid48561725600en_US
dc.contributor.authorid57188558332en_US
dc.date.accessioned2023-05-29T07:25:47Z
dc.date.available2023-05-29T07:25:47Z
dc.date.issued2019
dc.description.abstractThe effect sintering parameters and various amounts of additives on the TiO2-HA-CaSiO3 composites was investigated this study. TiO2/CaSiO3/HA composites were prepared and characterized by means of physical and mechanical properties. The addition of TiO2 and HA to wollastonite was studied by means of bulk density and Vickers Hardness. The wollastonite composites containing TiO2 (10-30 wt%) and HA (20-40 wt%) were sintered between 1230-1270�C, with a ramp rate of 10�C/min and a holding time of 1,1.5 and 2 hours. The results indicate that a higher sintering temperature played a significant part in enhancing the physical and mechanical properties as compared to results shown by pure wollastonite, especially for composites containing higher TiO2 (25-30wt%) and lower HA (20-25wt%). � BEIESP.en_US
dc.description.natureFinalen_US
dc.identifier.epage261
dc.identifier.issue7
dc.identifier.scopus2-s2.0-85067846524
dc.identifier.spage259
dc.identifier.urihttps://www.scopus.com/inward/record.uri?eid=2-s2.0-85067846524&partnerID=40&md5=0bcc8592394b94040f26bf7c348124df
dc.identifier.urihttps://irepository.uniten.edu.my/handle/123456789/24677
dc.identifier.volume8
dc.publisherBlue Eyes Intelligence Engineering and Sciences Publicationen_US
dc.sourceScopus
dc.sourcetitleInternational Journal of Innovative Technology and Exploring Engineering
dc.titleThe effect of holding time on the mechanical and physical properties of titania-wollastonite-hydroxyapatite compositesen_US