Publication: Failure evaluation on a high-strength alloy SA213-T91 super heater tube of a power generation
dc.citedby | 5 | |
dc.contributor.author | Ahmad J. | en_US |
dc.contributor.author | Purbolaksono J. | en_US |
dc.contributor.author | Beng L.C. | en_US |
dc.contributor.author | Ahmad A. | en_US |
dc.contributor.authorid | 57210531371 | en_US |
dc.contributor.authorid | 8621252500 | en_US |
dc.contributor.authorid | 26423491900 | en_US |
dc.contributor.authorid | 57214160450 | en_US |
dc.date.accessioned | 2023-12-29T07:49:09Z | |
dc.date.available | 2023-12-29T07:49:09Z | |
dc.date.issued | 2010 | |
dc.description.abstract | This article presents failure investigation on a high-strength alloy SA213-T91 super-heater tube. This failure is the first occurrence involving the material in Kapar Power Station Malaysia. The investigation includes visual inspections, hardness measurements, and microscopic examinations. The failed super-heater tube shows a wide open rupture with thin and blunt edges. Hardness readings on all the as-received tubes are used for estimating the operating metal temperature of the super-heater tubes. Microstructures of the failed tube show numerous creep cavities consisting of individual pores and chain of pores which form micro- and macro-cracks. The findings confirmed that the super-heater tube is failed by short-term overheating. Higher temperatures of the flue gas due to the inconsistent feeding of pulverized fuels into the burner is identified to cause overheating of the failed tube. | en_US |
dc.description.nature | Final | en_US |
dc.identifier.doi | 10.1243/09544089JPME332 | |
dc.identifier.epage | 273 | |
dc.identifier.issue | 4 | |
dc.identifier.scopus | 2-s2.0-78049477515 | |
dc.identifier.spage | 269 | |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?eid=2-s2.0-78049477515&doi=10.1243%2f09544089JPME332&partnerID=40&md5=e7ff51851bd11191a3943cf7924f89f8 | |
dc.identifier.uri | https://irepository.uniten.edu.my/handle/123456789/30541 | |
dc.identifier.volume | 224 | |
dc.pagecount | 4 | |
dc.publisher | SAGE Publications Ltd | en_US |
dc.source | Scopus | |
dc.sourcetitle | Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering | |
dc.subject | failure analysis | |
dc.subject | hardness measurements | |
dc.subject | high-strength alloy steel | |
dc.subject | micro-structure examinations | |
dc.subject | overheating | |
dc.subject | Alloy steel | |
dc.subject | Failure (mechanical) | |
dc.subject | Failure analysis | |
dc.subject | Hardness | |
dc.subject | High strength steel | |
dc.subject | Microstructure | |
dc.subject | Outages | |
dc.subject | Pulverized fuel | |
dc.subject | Tubes (components) | |
dc.subject | Failure investigation | |
dc.subject | Hardness measurement | |
dc.subject | Metal temperature | |
dc.subject | Micro and macro | |
dc.subject | overheating | |
dc.subject | Power station | |
dc.subject | Short-term overheating | |
dc.subject | Visual inspection | |
dc.subject | High strength alloys | |
dc.title | Failure evaluation on a high-strength alloy SA213-T91 super heater tube of a power generation | en_US |