Publication: Effect of holding time on the mechanical properties and microstructural evaluation of 3Y-TZP ceramics
No Thumbnail Available
Date
2017
Authors
Golieskardi M.
Satgunam M.
Ragurajan D.
Journal Title
Journal ISSN
Volume Title
Publisher
Springer International Publishing
Abstract
The extensiveness of additives such as CeO2 and Al2O3 in enhancing the mechanical properties of 3 mol% yttria-stabilized tetragonal zirconia polycrystalline (3Y-TZP) is examined. The samples are sintered at temperature ranging from 1250 to 1550 �C for different holding time of 12 mins and 2 h. The optimum amounts of dopants and sintering time are 0.5 wt% CeO2/0.3 wt% Al2O3 and 2 h, respectively. At these optimum conditions, the doped 3Y-TZP ceramic samples exhibit density of 5.96 g/cm3, Vickers hardness of 10.9 GPa, fracture toughness of 10 MPa.m1/2, Young's modulus of 238 GPa, and flexural strength of 750 MPa. � 2017 Australian Ceramic Society.
Description
Ceramic materials; Doping (additives); Elastic moduli; Fracture toughness; Sintering; Vickers hardness; Yttria stabilized zirconia; Zirconia; 3Y-TZP; Ceramic samples; Holding time; Microstructural evaluation; Optimum conditions; Polycrystalline; Sintering time; Yttria stabilized tetragonal zirconias; Mechanical properties